Tank Information
Diameter = 60m
Internal Design Pressure = 1.62kPa
Roof = Supported Cone
Roof Slope = 9º
The client is requesting that the tank roof be frangible. The tank meets the frangibility requirements per 5.10.2.6, with maybe the exception of the compression ring type.
The Appendix F.5.1 calculation results in a large compression area required and it is difficult to get the required compression area using Fig F-2 details a-e.
1) Is it the intention of figure F-2 that standard structural angles be used?
2) Can a large fabricated angle (eg. 300 x 300 x 25) be used to meet the frangibility requirements and gain the area required, keeping within the wc and Le limits?
Thanks
Diameter = 60m
Internal Design Pressure = 1.62kPa
Roof = Supported Cone
Roof Slope = 9º
The client is requesting that the tank roof be frangible. The tank meets the frangibility requirements per 5.10.2.6, with maybe the exception of the compression ring type.
The Appendix F.5.1 calculation results in a large compression area required and it is difficult to get the required compression area using Fig F-2 details a-e.
1) Is it the intention of figure F-2 that standard structural angles be used?
2) Can a large fabricated angle (eg. 300 x 300 x 25) be used to meet the frangibility requirements and gain the area required, keeping within the wc and Le limits?
Thanks