In a paper converting mill, one of our draw roller shaft failed at the weakest point (near the bearing and chamfer with the radius of 0.5). Rachet marks (but shiny) indicates that fatigue cracks were initated at a few locations along the groove. The eccentric pattern tells me that the load on the shaft was imbalanced BUT it's only pressing on tissue papers, and to our knowledge, there was no excessive loads. Two shafts failed within a month... it's really frustrating.