Can anyone explain the following:
copper 1/4 Hard
copper 1/2 Hard
copper 4/4 Hard
The above are used in a strain formula I am using. Basically, in the formula you would use a permissible strain of 1200daN/cm^2 for 1/4, 2300 for 1/2, and 3000 for 4/4.
Problem is, the manufacturer has given the hardness of the copper I am using as a hardness of 84 from a rockwell Hardness test?
How do I get the 2 to meet?