obrien0403
Civil/Environmental
I have a project that requires all the roadway fill to have less than 35% passing the 200 sieve. The plant asphalt roadway pavement design is a CBR of 1. The fill depth is about 5' and is compacted to 100% standard.
The on site materials have about 50% passing the 200 sieve. The geotechnical engineer has approved the deviation and will allow the 50% passing material. The owner wants the 35% passing material (or a credit).
One option I am considering is to mix the on-site material with sand to lower the 50% to 35%. It would be blended with a dozer.
By doing this is the material any better ?
What are the engineering concerns with too much material passing the 200 sieve ?
The on site materials have about 50% passing the 200 sieve. The geotechnical engineer has approved the deviation and will allow the 50% passing material. The owner wants the 35% passing material (or a credit).
One option I am considering is to mix the on-site material with sand to lower the 50% to 35%. It would be blended with a dozer.
By doing this is the material any better ?
What are the engineering concerns with too much material passing the 200 sieve ?