Riveting Nylon?

Status
Not open for further replies.

Cowboy67

New member
Apr 4, 2005
1
Is it advisable to use driven rivets to attach nylon parts to aluminum structure? If the nylon parts are picking up structural rivets is there any loss of strength in the rivet joint?
Thanks
 
Replies continue below

Recommended for you

Rivets are a suitable fastener for nylon mouldings provided they have some clearance in the hole, and the nylon is moisture conditioned before the riveting.