Jan 26, 2007 #1 draftsman101 Aerospace Joined Dec 3, 2006 Messages 149 Location US I am looking for the standards on what rivet lengths to use.
Jan 26, 2007 #2 Vroaar New member Joined Jan 26, 2007 Messages 1 Location US The short answer: the protruding shaft length = 1.5 x the rivet diameter. Before setting the rivet of course. The long answer: check out the AC 43.13-1b at FAA.gov. Upvote 0 Downvote