Can someone please tell me what the part number is for rivet code DH 4? Or where I can find it? Thank you.
 
You'll find the letter codes in NAS523. DH is an MS20427F (stainless steel rivet). The 4 indicates diameter (1/8).

You'll have to determine rivet length on installation.
 