Hand wheel operated Rising Stem Globe not rotating, when checked Stem got locked with Yoke Bush. Material Stem ASTM A410 Type 410, Yoke Bush A582 Type 416
Will it be due to dust entry into Stem thread.
Will it be due to thread damage due to excess torque
Will it be due to differential expansion of Stem & Yoke Bush thread
Could anybody guide me in finding out probable cause of failure
Will it be due to dust entry into Stem thread.
Will it be due to thread damage due to excess torque
Will it be due to differential expansion of Stem & Yoke Bush thread
Could anybody guide me in finding out probable cause of failure