Hello I am running a f1 4020 6000w co2 amada laser I am having issues where after my sharp corners I get ripples on my .25 .38 and .50 hrs steel I have tried the recovery but I am having trouble all my holes are coming out great and after about an inch it smooths back out but it just can't seem to recover anyone have any suggestions out there?
 