Have retaining wall on residential property. “2 blocks high” at one end, 9 ft high at the other - curves around corner of house – double deep in one area (on a slope). I do not believe drainage was done properly. There are no “weep holes” and there is not an area below that allows water to exit from behind the wall. There is a culvert below the ground that it might be tied into. Retaining wall is separating in two areas with gaps of 5 to 6 inches between upper and lower block. Cap blocks are disintegrating as well.
Due to drainage and wall failure, corner of house is "dropping" and creating cracks in walls and ceiling inside the home as well as the cinder block in two different areas outside.
There is no record of a permit from the city (required) and the company will not reply to my emails to even a general inquiry about the wall or even the manufacturer of the block. Former home owner had it built, and rebuilt at least one time. Wall is 12+ years old.
Wondering if contractor would be responsible being a permit wasn’t pulled for the damage that is being done to the house as well as rebuilding the wall properly. I live in MN.
Appreciate any help provided – or a direction I can go. $20,000+ for a new wall, my insurance won’t even look at it unless we dig the wall out and expose the corner of the house that is sinking.
Please help! Thank you in advance
Have retaining wall on residential property. “2 blocks high” at one end, 9 ft high at the other - curves around corner of house – double deep in one area (on a slope). I do not believe drainage was done properly. There are no “weep holes” and there is not an area below that allows water to exit from behind the wall. There is a culvert below the ground that it might be tied into. Retaining wall is separating in two areas with gaps of 5 to 6 inches between upper and lower block. Cap blocks are disintegrating as well.
Due to drainage and wall failure, corner of house is "dropping" and creating cracks in walls and ceiling inside the home as well as the cinder block in two different areas outside.
There is no record of a permit from the city (required) and the company will not reply to my emails to even a general inquiry about the wall or even the manufacturer of the block. Former home owner had it built, and rebuilt at least one time. Wall is 12+ years old.
Wondering if contractor would be responsible being a permit wasn’t pulled for the damage that is being done to the house as well as rebuilding the wall properly. I live in MN.
Appreciate any help provided – or a direction I can go. $20,000+ for a new wall, my insurance won’t even look at it unless we dig the wall out and expose the corner of the house that is sinking.