rms1956

Materials
Jul 23, 2001
17
I'm looking for articles/papers on retained autenite in 17-7PH SS. Particularly interested in articles/papers contianing photos of evidence in the microstructure.

Thanks
 
Replies continue below

Recommended for you

17-7 has a very complex microstructure, in the annealed form I am certain its mostly austenitic. When heat-treated to eitehr RH or TH conditions I would expect that the structure still contains significant austenite.

Also I'd expect convesely that CH condition material is completely martensitic.


Nick
I love materials science!
 
I just took a look at some old 17-7 CH900 micros I had and there is perhaps 10-15% of a lighter etching phase. If memory serves me correct, this is delt ferrite.
 
Thanks, I did start a bit of research into 17-7, but working in a more production environment stalled the research, all the samples are ready an labled, but I never really was able to start the next steps. Ugh..
 
Retained austenite seems to be everywhere !! It can be found in low carbon martensite and even bainite ! Now that we can get to 1,000,000X we can see lots of things like G-P zones and dislocations !
 