Hi~

Once I found that resistivity of p-type Si is 7.8e-8 T??m, is it equal to 7.8?cm?
 
Replies continue below

Recommended for you

T=Terra=10e12 then you're right...but not every p-doped Si has this specific resistivity...it depends on the implanmtation treatment

 