Apr 23, 2009 #1 dik Structural Joined Apr 13, 2001 Messages 26,116 Location CA I'm looking for a quick drying coating to resist Dimethylamine (dangerous stuff). thanks, Dik
Apr 23, 2009 #2 Compositepro Chemical Joined Oct 22, 2003 Messages 7,841 Location US Epoxy would probably work well. Dimethylamine is a curing agent for epoxy. Upvote 0 Downvote
Apr 24, 2009 Thread starter #3 dik Structural Joined Apr 13, 2001 Messages 26,116 Location CA Thanks... we'll look into epoxy primers and epoxy topcoats. Dik Upvote 0 Downvote