Somebody could suggest me any tutorial or text about residual stress on welding analysis or only residual stress on pro/mechanica?

thanks in advance

Edited by: AragornPE
 
Try this as an starter. There might be some more recent books avalable on subject.

Analysis of Welded Structures: Residual Stresses, Distortion, and Their Consequences
Koichi Masubuchi
# Hardcover: 600 pages
# Publisher: Pergamon Pr; 1st ed edition (May 1980)
# Language: English
# ISBN: 0080227147
 