Hi,
we are trying to take the replica of U duct made up of INCONEL material. What is the most appropriate etchant for INCONEL Alloys?
What are the possible phases and microsturcture and which damage mechanisms may occur to this alloy?
Please help.
 
Replies continue below

Recommended for you

Which alloy? Inconel is the tradename for a family of dozens of Ni based alloys.

= = = = = = = = = = = = = = = = = = = =
P.E. Metallurgy, Plymouth Tube
 
Metallurgist 1991;

First, you can search on your own and find plenty of information on microstructure and associated damage mechanisms. See below to name a few


Another


Second, regarding etching behavior, see the link below

 