Like most water utilities, we have some asbestos cement (AC) pipe in our distribution system, mostly in the 4"-10" range. We are looking to replace some in the near future and are looking at construction methods, risks, and responsibilites. We are lookinig at possibly totally abandoning the old ac main and replacing with new pipe. We are also looking at main bursting with a larger diameter pipe which will leave fragments of the ac pipe in place. The last alternate and most expensive is total removal and proper discarding of the ac pipe. There are risks associated with each alternate, as well as different costs. Does anyone have any information that you can provide regarding recommened replacement methods or responsible construction methods, etc.? Any information will be greatly appreciated.