We use SS305 for certain components. For cost reduction, I am planning of using SS204Cu, or maybe SS201.
But with the higher strength of SS201, would I need to modify the tooling?
I would like to use the same set of tools.
Strength is not important for my requirement, I require low magnetic permeability.
What do you suggest?
Also, what is a reliable site to get a rough estimate of stainless steel prices? I am looking for SS434, 400, 201