What are the implications from switching from a Tube Steel member, and using steel plate to build the section as a weldment assembly (other than the lower yield stress).
 
Replies continue below

Recommended for you

For starters:

Higher Cost of fabrication.

Weld quality.

Appearance.



Mike McCann
MMC Engineering
Motto: KISS
Motivation: Don't ask
 