repairs to pre-stressed concrete piles

Status
Not open for further replies.

Prepakt1

Coastal
Joined
Mar 30, 2004
Messages
155
Location
CA
Has anyone done repairs to prestressed piles suffering from spalding and corrosion. This if for a Jetty in Lybia. What method have you userd and results. We can use pile jackets is there any other method that can privide a good repair.

 
Hi Prepakt1

Try epoxy coated glass fibre wrap. For piles these would mainly be used to maintain confinement. Check with Hexcel Fyfe or other such similar companies.

Regards

VOD
 