Hi all

Can anybody help with my question below:

If Sec 8.1.6.4.2 (Preheat or Controlled Deposition Welding Methods as Alternatives to Postweld Heat Treatment) of API 510 was followed instead of doing a PWHT for a repair on a vessel that was originally stress relieved, will it change the vessel’s HT status?

Thanks,

 
No. The vessel had been originally heat treated for ASME Code compliance. What happens to the vessel in service is another code's responsibility - NBIC or API 510, and ASME does not care after the vessel is in service.
 
I mean if we need to remove the HT stampe on the Nameplate and if we need to re-register with ABSA.
 
Doing a repair to a Code Vessel in Alberta requires working with ABSA prior to performing the repair. They'll guide you through the process.
 