I have read somewhere that some steelmakers introduce nitrogen in the steel molten and after the vacuum refining process and degassing the nitrogen will form bubbles. The degassing of these bubbles take with them some dissolved hydrogen
1- Is that True?
2 -Anyone have some informations about this
Thanks
Stan