Dear All,
Tubular heat exchanger in our plant we use to produce purified and process water(high temperature) for about 5years but, now condensate leakage is visible at the inner tube plate due to the failed sealing off between tube and plate. Because of the special running condition under which the prw(production water) formulation doesn't need continually water supplying, therefore the heat exchanger always stars intermittently and cause shell temperature varying and the expansion stress cause the gaps at the sealing point of inner rube plate and tube bundle.
How to repair this leakage?
Thanks and Reagards
zhangbd
Tubular heat exchanger in our plant we use to produce purified and process water(high temperature) for about 5years but, now condensate leakage is visible at the inner tube plate due to the failed sealing off between tube and plate. Because of the special running condition under which the prw(production water) formulation doesn't need continually water supplying, therefore the heat exchanger always stars intermittently and cause shell temperature varying and the expansion stress cause the gaps at the sealing point of inner rube plate and tube bundle.
How to repair this leakage?
Thanks and Reagards
zhangbd