A 3000 RPM generator was out of service for two years. Since the utility owner did not use keeper plates, the rotating permanent magnets of the PMG (whose output supplies the AVR) lost some of its magnetism. During recommissioning the generator, the PMG output voltage was only 1/3rd of its rated voltage and hence the AVR is not working.
Any ideas/suggestions on how to restore the magnetism of these rotating permanent magnets would be greatly appreciated.
A photo of the PMG rotor.
Muthu
Any ideas/suggestions on how to restore the magnetism of these rotating permanent magnets would be greatly appreciated.
A photo of the PMG rotor.

Muthu