Is there a requirement in ASME Code to use reinforcing pad plates at nozzles > 2"?

I'm planning a pressure vessel in Stainless Steel Dia 3m, pressure 11 barg.

Thanks for your replies

Regards
UliR
 
NO, see UG-27 and UW-16,
depends on the thickness of the vessel and t of the nozzle,
you have to run calcs for compensation, if compensation is required, you may add to the weld size weld design or a pad.
ER
 
One must also consider loading from connected piping (UG-22), and this can sometimes lead to requirement for additional reinforcement at the nozzle.
 
Gents,

thanks for your replies, they were helpfull for my planning

Best regards
UliR
 
There is no requirements depending of the t of the vessel there can be restrictions,
reinforcing may be required on the welds or a particular size of weld throat. if you are not sure, it is best eng practice to run calcs.
see uw16 for exceptions
ER
 
generalblr and JohnGP had the best answer. I hope to introduce an example;
External load (force and moment for process nozzles) may require the repad (e.g., in WRC 107 calculation) even if UG-36 permits no-repad for small size nozzle opening.
Even though we use the LWN type for 1 1/2" or 2" nozzles, the repads are sometimes required additionally due to the external piping force and moment given by client.
 