Hi,

Does anyone know if there is anything in the ACI limiting the reinforcement ratio in a collector? Section 18.12.7.5 of ACI 318 references SMF column requirements of sections 18.7.5.2(a)-(e) and 18.7.5.3. The SMF column 6% requirement is referenced in 18.7.4.1.

Thanks
 
Replies continue below

Recommended for you


ACI 318 does not suggest max. reinforcement ratio in a collector longitudinal reinforcement . But constructability may be issue. If congestion impede placement of concrete and ultimate performance, increasing the dia of reinf . and the slab depth are the applicable options.

Pls look Section 9. Detailing and Constructability Issues of the following doc.
...

He is like a man building a house, who dug deep and laid the foundation on the rock. And when the flood arose, the stream beat vehemently against that house, and could not shake it, for it was founded on the rock..

Luke 6:48

 
 https://files.engineering.com/getfile.aspx?folder=9bc58783-3e2d-489e-865a-9ef6ed508084&file=NIST.GCR.16-917-42_Concrete_Diaphragms,_Chords,___.pdf
Status
Not open for further replies.

Part and Inventory Search

Sponsor