Does anyone know where I can find "hammertone" material? I think that is what it is called. Being used as a reflector material to diffuse light. I believe it is aluminum and essentially has a dimpled surface appearance.
 
Hello Jade,

What application will you use for this reflector, spot light, Projector light, torch......?
It will use different materials for heat resistance purpose. Normally, the surface is coated with aluminum.

Raymond Law
 