I'm trying to find information on reflective cracking control with Superpave pavements. I have heard that Superpave, because of its more consistent properties while cold and improved properties in tension, reduces the rate of reflective cracking but can't find anything on it. Does anybody know the difference between Marshall and Superpave mixes as far as that?
Thanks in advance...