Good day! I have a question in regards to ball valves.
I just took over a project for a Process Plant and I'm checking the selection of valves. When I came to ball valves 600# our specification says to be "Reduced Bore" but our three vendors (all very well known and respected) had offered "Full Bore".
Is this standard for 600#?
Thanks for your help!
 
Replies continue below

Recommended for you

caihui,
Sorry to say this time you are wrong... at least in respect with the spec...

We specify (bearing in mind this spec is 8 years old!) BS5351 Ball Valves Reduced Bore 600#.

I don't have any objection with full bore valves for this application (process plant... no pigging, no probe going trough, etc.. only shut on-off valve) but I got three different offers for a Full Bore valve (from three different manufacturers) and I was wondering whether the "standard practice" had changed (and so should my specification) or it was more an economical issue.


I thank you all guys for your answers (it was much more than I expected, as I also learnt/refreshed some other things beside my question)
 
Morten,

No worries.

"Do not worry about your problems with mathematics, I assure you mine are far greater."
Albert Einstein
Have you read FAQ731-376 to make the best use of Eng-Tips Forums?
 
Status
Not open for further replies.

Part and Inventory Search

Sponsor