How can we reduce the linear expansion of a molded part, once molded? It is 6/6 nylon.
I understand fiberglass reinforced 6/6 nylon would not expand as much, yet we have stock that is just 6/6 nylon.
Are there any treatments that could help to reduce the amount of linear expansion when elevated to higher temperatures like from 70 F to 110 F?
Any input is very welcome
Thanks, John
I understand fiberglass reinforced 6/6 nylon would not expand as much, yet we have stock that is just 6/6 nylon.
Are there any treatments that could help to reduce the amount of linear expansion when elevated to higher temperatures like from 70 F to 110 F?