I have attached a sketch to show the situation. Basically we need to split a shell due to manufacturing reasons at the location of an internal plate. Can anyone give a recommendation on the type of weld to use to at the joint?
This is an ASME VIII Div.1 vessel. The shell OD is 22 in so it is possible to get inside to add an internal fillet weld on the open end.
Has anyone encountered this situation before?
What is of concern is that if shell sections are attached by full pen "V" groove weld full penetration, the shell sections would be reliably joined, but the flat plate will have welding only around its outer edge. Not ideal to me!
Thanks
I have attached a sketch to show the situation. Basically we need to split a shell due to manufacturing reasons at the location of an internal plate. Can anyone give a recommendation on the type of weld to use to at the joint?
This is an ASME VIII Div.1 vessel. The shell OD is 22 in so it is possible to get inside to add an internal fillet weld on the open end.
Has anyone encountered this situation before?
What is of concern is that if shell sections are attached by full pen "V" groove weld full penetration, the shell sections would be reliably joined, but the flat plate will have welding only around its outer edge. Not ideal to me!