Piper AlphaGas audibly leaked out at high pressure, drawing the attention of several men and triggering six gas alarms including the high level gas alarm. Before anyone could act, the gas ignited and exploded, blowing through the firewall made up of 2.5 × 1.5 metre panels bolted together, which were not designed to withstand explosions. The custodian pressed the emergency stop button, closing huge valves in the sea lines and ceasing all oil and gas production.
Theoretically, the platform would then have been isolated from the flow of oil and gas and the fire contained. However, because the platform was originally built for oil, the firewalls were designed to resist fire rather than withstand explosions. The first explosion broke the firewall and dislodged panels around Module (B). One of the flying panels ruptured a small condensate pipe, creating another fire.
10:04 p.m. The control room was abandoned. Piper Alpha's design made no allowances for the destruction of the control room, and the platform's organisation disintegrated. No attempt was made to use loudspeakers or to order an evacuation.
Emergency procedures instructed personnel to make their way to lifeboat stations, but the fire prevented them from doing so. Instead the men moved to the fireproofed accommodation block beneath the helicopter deck to await further instructions. Wind, fire and smoke prevented helicopter landings and no further instructions were given, with smoke beginning to penetrate the personnel block.
As the crisis mounted, two men donned protective gear in an attempt to reach the diesel pumping machinery below decks and activate the firefighting system. They were never seen again.
The fire would have burnt out were it not being fed with oil from both Tartan and the Claymore platforms, the resulting back pressure forcing fresh fuel out of ruptured pipework on Piper, directly into the heart of the fire. The Claymore platform continued pumping until the second explosion because the manager had no permission from the Occidental control centre to shut down. Also, the connecting pipeline to Tartan continued to pump, as its manager had been directed by his superior. The reason for this procedure was the exorbitant cost of such a shut down. It would have taken several days to restart production after a stop, with substantial financial consequences.
Gas pipelines of both 16″ and 18″ diameter ran to Piper Alpha. Two years earlier Occidental management ordered a study, the results of which warned of the dangers of these gas lines. Due to their length and diameter, it would have taken several hours to reduce their pressure, so that it would not have been possible to fight a fire fueled by them. Although the management admitted how devastating a gas explosion would be, Claymore and Tartan were not switched off with the first emergency call.
10:20 p.m. Tartan's gas line (pressurised to 120 Atmospheres) melted and burst, releasing 15-30 tonnes of gas every second, which immediately ignited. From that moment on, the platform's destruction was assured.
10:30 p.m. The Tharos, a large semi-submersible fire fighting, rescue and accommodation vessel, drew alongside Piper Alpha. The Tharos used its water cannons where it could, but it was restricted, because the cannons were so powerful they would injure or kill anyone hit by the water.
10:50 p.m. The second gas line ruptured (the riser for the MCP-01 platform), ejecting millions of cubic feet of gas into the conflagration. Huge flames shot over 300 ft (90 m) in the air. The Tharos was driven off by the fearsome heat, which began to melt the surrounding machinery and steelwork. It was only after this second explosion that the Claymore platform stopped pumping oil. Personnel still left alive were either desperately sheltering in the scorched, smoke-filled accommodation block or leaping from the various deck levels, including the helideck, some 175 ft (50 m) into the North Sea. The explosion also killed two crewmen on a fast rescue boat launched from the standby vessel Sandhaven and the six Piper Alpha crewmen they had rescued from the water.[4]
11:20 p.m. The gas pipeline connecting Piper Alpha to the Claymore Platform burst.
11:50 p.m. The generation and utilities Module (D), which included the fireproofed accommodation block, slipped into the sea. The largest part of the platform followed it.
12:45 a.m., 7 July The entire platform had gone. Module (A) was all that remained of Piper Alpha.
At the time of the disaster 226 people were on the platform; 165 died and 61 survived.[10] Two men from the Standby Vessel Sandhaven were also killed.
We have several recip compressors running in an onshore oil production/gas injection facility. The condition of starting up the compressors loaded or unloaded depends on the 1st stage suction/discharge pressure because of (as BigInch and DLite30 said) the starting torque requirements. Have a look to the compressor's operating manual. At any trip we blowdown the compressors to avoid condensation in the lines (wet gas). The amount of gas lost is negligible when compared to the problems we could have getting liquids inside the cylinder.