97EOs
Civil/Environmental
- May 15, 2013
- 3
Does anyone own a Rebound Hammer? Have you tried testing it on a 1000 psi, 2000 psi, 3000 psi, 4000 psi, 5000 psi concrete to see if the results correlate supposing the surface is even and representative of the concrete? I saw it done and it seems to correlate somewhat.