Tek-Tips is the largest IT community on the Internet today!

Members share and learn making Tek-Tips Forums the best source of peer-reviewed technical information on the Internet!

  • Congratulations cowski on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Rebar Weight 2

Status
Not open for further replies.

mjohan

Structural
Joined
Dec 7, 2002
Messages
91
Location
US
What is the weight of a piece of rebar? (#3, #4, #5, #6, #7, and #8)

I am also curious as to the comparitive price/ lb of rebar to W steel beam shapes. Just trying to get a feel for the cost with the rising steel prices.

Thanks
 
Check the appendices to a steel handbook - also, I believe in AASHTO M31.
 
ACI318-99, appendix E lists rebar weights.
 
Vendors will send you a chart as well.

[pacman]

Please see FAQ731-376 for great suggestions on how to make the best use of Eng-Tips Fora. See faq158-922 for recommendations regarding the question, "How Do You Evaluate Fill Settlement Beneath Structures?"
 

#3 = .376 lbs/lf
#4 = .668 lbs/lf
#5 = 1.043 lbs/lf
#6 = 1.502 lbs/lf
#7 = 2.044 lbs/lf
#8 = 2.670 lbs/lf
#9 = 3.400 lbs/lf
#10 = 4.303 lbs/lf
#11 = 5.313 lbs/lf
 