Greatone76
Structural
- Feb 2, 2006
- 64
I have a situation were it has come to light on the job I'm doing inspection work for that the contractor placed (3) #5 rebar all in one plane at the bottom of a standard 8" stem wall with only a max of 5/8" spacing. Per ACI-318 the requirement is a minimum spacing of 1". I'm not the engineer for this project, I'm an owner's rep, but it appears that the CM is going to have the design engineer sign off on the situation. Since ACI-318 is the building code is it right to allow a sign off of code requirements. Am I wrong to be completely opposed to a sign off in this situation. I'm of the understanding that the concrete will separate aggregate and cream and not bond well to the rebar and could create voids ann/or a weak spot in the concrete in this area, so I would think this would be a critical issue. Please give me any advise or perspective on this issue.