Hello out there - I have an interesting question based on reality.
Suppose a home was built, with a suspended concrete slab. The architect/engineer specified #60 rebar on 12" centers, two layers offset 6" (not technically correct, but you get the picture).
Suppose the guy pouring the slab used #40 rebar (40ksi).
What are the possible failures, etc?
It is the garage floor of a home.
Thanks.
Suppose a home was built, with a suspended concrete slab. The architect/engineer specified #60 rebar on 12" centers, two layers offset 6" (not technically correct, but you get the picture).
Suppose the guy pouring the slab used #40 rebar (40ksi).
What are the possible failures, etc?
It is the garage floor of a home.