I'm confused why many Rebar benders on the market, and many I have seen used on construction sites, don't appear to meet the ACI recommendation for min bend diameter.
I was recently on a job that used a Rebar bender similar to this one:
The resulting bend on a #4 bar was slightly less than a 1 inch diameter, a far cry from the recommended 3". Is there any explanation for why these products don't meet the specification, is there some detail I'm missing or are they just ignoring the standard?
The majority of jobs in my area use Rebar benders similar to this one. The building inspector signs off on these jobs, so that is where my confusion comes from.
I was recently on a job that used a Rebar bender similar to this one:
The resulting bend on a #4 bar was slightly less than a 1 inch diameter, a far cry from the recommended 3". Is there any explanation for why these products don't meet the specification, is there some detail I'm missing or are they just ignoring the standard?

The majority of jobs in my area use Rebar benders similar to this one. The building inspector signs off on these jobs, so that is where my confusion comes from.