Tek-Tips is the largest IT community on the Internet today!

Members share and learn making Tek-Tips Forums the best source of peer-reviewed technical information on the Internet!

  • Congratulations MintJulep on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Reasons why Aluminium alloy is not used for plastic extruder barrel material ? 1

Status
Not open for further replies.

Uralsk

Mechanical
Joined
Feb 21, 2021
Messages
39
Location
ID
I wondered why aluminium alloy is not used for plastic extruder barrel material ?
Is it mainly because of the galling resistance of aluminium alloy ?
What is the other factors that aluminium alloy is not suitable for plastic extruder barrel?
Also i'm planning to use aluminium silicon alloy grade that is used for car engine block which i heard is the most galling resistant grade of all aluminium alloys.
 
You certainly have asked similar questions more than a dozen times but I don't know why you ask.

Aluminum isn't used because it isn't the best material for the function.

That should not prevent you from placing an order with an extruder screw company and telling them it needs to be some alloy of aluminum. I'm sure any extruder screw company will be happy to take your money to make one. When they deliver it they will block you telephone number because they don't want you asking why it snapped in half when you used such a weak material. More than likely - they will block your number as soon as you say "aluminum."
 
Sorry for asking a many times because I'm not fully sure about it
Also i wanted to know what is the main disadvantages other than galling and how many disadvantages point list?
 
Sorry for asking a many times because I'm not fully sure about it
Also i wanted to know what is the main disadvantages other than galling and how many disadvantages point list?

You seem to be obsessed with galling; you should be looking to see what other materials are actually being used and compare their material properties, or better yet, READ the literature and advertising

TTFN (ta ta for now)
I can do absolutely anything. I'm an expert! faq731-376 forum1529 Entire Forum list
 
High thermal expansion makes keeping needed tolerances difficult.
Low wear resistance is a issue with any filled polymer causing excessive erosion.
Limited strength at elevated temperatures may require design changes.
Plenty of other negatives beyond galling resistance.

= = = = = = = = = = = = = = = = = = = =
P.E. Metallurgy, consulting work welcomed
 
FWIW, here's ChatGPT's take on your problem; note that aluminum didn't even make it to the top 5 materials. I think that even diamond would top aluminum on the list

Note that OpenAI explicitly mentions that ChatGPT can give out wrong information

chat_nozzle_vxuiwl.png


TTFN (ta ta for now)
I can do absolutely anything. I'm an expert! faq731-376 forum1529 Entire Forum list
 
IRS... is that a reply by AI? If it is, Wow...

-----*****-----
So strange to see the singularity approaching while the entire planet is rapidly turning into a hellscape. -John Coates

-Dik
 
Chat GPT has made it as far as a marketing or sales level conversation. This has ZERO engineering value.

And it's obvious because it makes no mention galling issues of all of the materials recommend (well silicon carbide has other issues than galling).

We have created an artificial politician.... yay.
 
I didn't say it has engineering value... on first glance, it's quite a package; it had no idea that it had that capability. I'm trying to get my old Win 7 machine up and running (don't know why it stopped) where I have Delphi installed... to compile the Travesty program I just downloaded. I've ocr'ed the above clip and have the text file... I want to try running it through travesty just to see what comes out of the sausage machine...

-----*****-----
So strange to see the singularity approaching while the entire planet is rapidly turning into a hellscape. -John Coates

-Dik
 
Barrels and nozzles are not the same thing. The nozzle is at the end of the barrel.
 