if a heat treated joint is found to be faulty aftr radiography,after removing the discontinuity by grinding
and refilling by welding(only the faulty thickness) should i need to re-PWHT the whole joint even if the repaired thickness is less than 38 mm for P no1 material according to UCS56
THANK YOU
 
Replies continue below

Recommended for you

It all depends on the repair and the reasons for the original PWHT.

If the repair was of small depth (I do not have a code book with me so will go on memory) less than 1/2" (12mm) and the repair was performed with proper preheat and heat maintanence, then it may not have to be pending user and AI approval.

If the vessel was PWHT because of a process reason, it will be up to the USER to approve a repair procedure or to decide if a total local PWHT is in order.

in matters such as this, there are many factors to be considered. Our first action after finding a required repair after PWHT would be to write an NCR and get the AI, USER, and both mechanical & process engineers involved.

If it is a requirement to radiograph seams after PWHT, it is our standard to ultrasonic examine joints prior to PWHT to locate any possible repairs beforehand.
 