Hello,
I have a question about passive layer in the pipeline of 316L ss ? I have a demi water loop (water velocity is over 1.1 m/s, conductivity is about 0.5 uS, temp. about 20 deg C). As I know the thickness of passive layer is about couple particles. Is that possible the water after some time breaks off (wash up) the layer ?
Is that recommended to make a repassivation the ss surface after some time ? If so, do you know some standard (i.e. ISO, ASTM etc.) that treats of ?
Thanks for your help.
Regards
I have a question about passive layer in the pipeline of 316L ss ? I have a demi water loop (water velocity is over 1.1 m/s, conductivity is about 0.5 uS, temp. about 20 deg C). As I know the thickness of passive layer is about couple particles. Is that possible the water after some time breaks off (wash up) the layer ?
Is that recommended to make a repassivation the ss surface after some time ? If so, do you know some standard (i.e. ISO, ASTM etc.) that treats of ?
Thanks for your help.