Hello to everyone, I am new in this forum.
I have a question about "raw material testing methods" for rubber industry??
 
Replies continue below

Recommended for you

Ok, I wanted to know;

What are the serious and needed parameters to evaluate the raw materials of compound, such as oils,fillers,small chemicals,antiozonants etc....
 
You need a fully equiped chemical laboratory to evaluate the chemicals in their original state plus and fully equiped physical test laboratory to determine rheometer cure times, viscosity, hardness, tensile, perhaps tear resistance, dynamic modulus, ozone resistance, etc.

At a minimum I would look for changes in rheometer cure times, viscosity, hardness, and tensile properties. Take a look at for more on rubber history and technology.
 
in the R.T.Vanderbilt rubber handbook you can see what to check on each raw material, in Rubber plants you check the Mooney Viscocity of the raw rubber and some more like the moisture of every powder, etc
 