The following is explain in Annex B of ASME B16.5-2003
Flange characteristics:
12’’ 600# in A182 Gr. F53 (Group n°2 material)
Conditions:
Internal Design pressure = 84,8 bar (not relevant for the calculation)
Design Temperature = 204°C (approx. 400°F)
Test temperature = 20°C (approx. 68°F)
By applying the formula (3) from ASME B16.5-2003 Annex B:
Pc = 97,2 barg (1410 psig)
Pr = 600 psi
S1 =minimum of the following (Group 2 material)
· 70% of Yield Strength at 100°F (40°C) = 0,7 x 80,06 = 56 ksi
· 70% of Yield Strength at T (204°C) = 0,7 x 60,82 = 42,6 ksi
· 1,25 times the allowable stress at T (204°C) = 1,25 x 30,17 = 37,7 ksi
Therefore, S1 = 37,7 ksi
Then PT = 600 x 37700 / 8750 = 2585 psig
Our problem is then: PT is not below Pc.
The table 2-2.8 gives the value we should find: we should find 1230 psig @ 400°F. Where is our mistake?
The most disturbing is that by doing the same method with a more standard material (A105), we manage to find the same results than in the Table 2-1.1 specific to A105.
So does anybody know why we do not find 1230 psig even though we follow the method? Does it come from another consideration as explained in B1.1?
Thanks for your help.
Bertrand
Flange characteristics:
12’’ 600# in A182 Gr. F53 (Group n°2 material)
Conditions:
Internal Design pressure = 84,8 bar (not relevant for the calculation)
Design Temperature = 204°C (approx. 400°F)
Test temperature = 20°C (approx. 68°F)
By applying the formula (3) from ASME B16.5-2003 Annex B:
Pc = 97,2 barg (1410 psig)
Pr = 600 psi
S1 =minimum of the following (Group 2 material)
· 70% of Yield Strength at 100°F (40°C) = 0,7 x 80,06 = 56 ksi
· 70% of Yield Strength at T (204°C) = 0,7 x 60,82 = 42,6 ksi
· 1,25 times the allowable stress at T (204°C) = 1,25 x 30,17 = 37,7 ksi
Therefore, S1 = 37,7 ksi
Then PT = 600 x 37700 / 8750 = 2585 psig
Our problem is then: PT is not below Pc.
The table 2-2.8 gives the value we should find: we should find 1230 psig @ 400°F. Where is our mistake?
The most disturbing is that by doing the same method with a more standard material (A105), we manage to find the same results than in the Table 2-1.1 specific to A105.
So does anybody know why we do not find 1230 psig even though we follow the method? Does it come from another consideration as explained in B1.1?
Thanks for your help.
Bertrand