Hi, here's a picture of a broken cap scew involved in an accident. We will call it the "F" bolt. Other bolts around are SS ASTM F593. Unfortunately, this only one does not have a stadard mark and nobody around know about it. Many manufacturer's charts have been viewed and no clue appears.
The question is: What is the bolt grade?
A simple magnetic test showed us a difference, the "F" bolt react to the magnet.
Look at the picture below.
Luc Perron, structural ingineer
Luc Perron, engineer
Unigec Experts-conseils
The question is: What is the bolt grade?
A simple magnetic test showed us a difference, the "F" bolt react to the magnet.
Look at the picture below.
Luc Perron, structural ingineer
Luc Perron, engineer
Unigec Experts-conseils