Hi Guys and Gals,

Any one know what was finaly selected and how well is it working for Mr Scipio? Thread # 407-118609 .

I need a Rag Layer pump selection for similar case - Heavy API 20 Crude Oil. Rag Layer in various Separators require recycle or blow down.

Thank you in anticipation

AC
 
Replies continue below

Recommended for you

Well Scipio is still around, so maybe he'll see this thread and reply.

Patricia Lougheed

******

Please see FAQ731-376: Eng-Tips.com Forum Policies for tips on how to make the best use of the Eng-Tips Forums.
 
Thank you Patricia,

If anyone can put in a word for me to him, too, that will be great!

Thanks,

AC
 
I am pretty familiar with this application. For rag layer pumping we usually use progressive cavity pump(PCP). PCP is the only(?) PD pump (positive displacement pump) which its capacity doesn't change because of decrease in viscosity. It makes PCP as the best option for rag layer pumping which has different percentage of water/oil and sand in it.
For low temperature application NBR is a good choice as stator. For high temperature applications Viton can be used as stator.
Hope this help.
 