Pylko, I respectfully disagree. Notching the top of a rafter to bear on the ridge beam creates a wedge between the bearing surface and a short line of grain, which is vulnerable to splitting with loss of bearing. It is generally a poor practice. Notching the bottom creates no such problem, so long al the level cut is fully supported by the plate. Also, notching the top creates the need for blocking.