Hi everybody,
the first time i know definition "Radius reduced transverse tensile test". Can you show me standard relavant this test.
 
Please review ASME Section IX QW-462.1
 
Hi Metengr,
QW-462.1 is reduced transverse tensile test not Radius reduced transverse tensile test.

I search to internet:
- A reduced transverse tensile test specimen assesses the tensile strength of the joint.
- A radius reduced transverse tensile test specimen assesses the tensile strength of the weld
metal.

I want to know metthod "A radius reduced transverse tensile" but i cannot find standard relavant this test.
 