Nov 19, 2011 #1 qaengineer1969 Mechanical Joined Dec 1, 2010 Messages 8 Location GB When sentencing radiographs to ASME B31.1 when you work out the size of the pore size. Do you use the thickness of the weld or the thickness of the material.
When sentencing radiographs to ASME B31.1 when you work out the size of the pore size. Do you use the thickness of the weld or the thickness of the material.
Nov 19, 2011 1 #2 metengr Materials Joined Oct 2, 2003 Messages 15,478 Location US The Note in the 2010 Edition of B31.1 in 136.4.5 specifies t as the thickness of the weld. Upvote 0 Downvote
Nov 19, 2011 #3 bernoullies123 Mechanical Joined Dec 30, 2009 Messages 203 Location AU Just to add, the note says it shall be taken from the thinnest weld of dissimilar weld thickness. Same note applies back to least 2004 version. Upvote 0 Downvote
Just to add, the note says it shall be taken from the thinnest weld of dissimilar weld thickness. Same note applies back to least 2004 version.