I've briefly looked in B31.1 and Section I and I think the answer is no; however, I'm going to ask just in case.
For P1 material (drums and tubes) where PWHT is being performed, is the requisite RT required to be performed after PWHT?
In my opinion, RT should be performed prior to PWHT for info and required after PWHT (in case an otherwise acceptable defect "opens up" from the heat cycle). Our internal documents reflect this (and have for many years) but I haven't been able to determine if it's a code requirement or not. From what I've seen so far it isn't.
I found in B31.3 that for P3, P4, and P5 (I think those are the materials), NDT is required to be performed after PWHT.
Anyway, if you know for sure that it is or isn't your help would be appreciated. It would be even more appreciated if you could point me to the relevant sections of the code.
-InspEngr
For P1 material (drums and tubes) where PWHT is being performed, is the requisite RT required to be performed after PWHT?
In my opinion, RT should be performed prior to PWHT for info and required after PWHT (in case an otherwise acceptable defect "opens up" from the heat cycle). Our internal documents reflect this (and have for many years) but I haven't been able to determine if it's a code requirement or not. From what I've seen so far it isn't.
I found in B31.3 that for P3, P4, and P5 (I think those are the materials), NDT is required to be performed after PWHT.
Anyway, if you know for sure that it is or isn't your help would be appreciated. It would be even more appreciated if you could point me to the relevant sections of the code.