Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations waross on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Radial Rivets

Status
Not open for further replies.

Jalipa

Materials
Jun 5, 2001
35
I want to read up about radial riveting

Particularly about

1) The process
2) Typical applications
3) Guidelines

Any pointers anyone?

Thank you

J
 
Replies continue below

Recommended for you

The process is variation of the orbital riveting technique that has been around for a while.
The difference is in the tool motion. The orbital is what it says it is and radial is rosette pattern.
We were quite successful in using the orbital machines for build in Aluminum ducts. The biggest advantage on our part was less protrusion of the rivet on the set end. It looked a lot better also.
It is my understanding that you get better sets with the radial. Smaller with full strength or spread out for a lower profile.

I would get on the net and contact several manufacturers, get there brochures and get some talking points concerning your intended use and then RFQ.
 