just looking for info to fill out qw-482 forms for

a 6 G position weld on 4" xxs pipe whith a grade

of api grade 5ax to 5ax
 
Try It doesn’t tell you how to fill out the form but it gives you all the essential variables and includes an approval range calculator.

A 5A material approves 5A to 5A and 5A to 4, 3 , or 1.

If you need blank copies of the form they ar on web site in .pdf format, free!!

Have fun
 