QW-407.2 ASME IX
I have a PQR with PWHT time range of 210 min.
I have a WPS with PWHT of 96 min. (time range is the minimum required acc. to ASME VIII Div.1)
Welds are impact tested.
Question: may I use that PQR to cover this WPS? (assuming all other variables ok)
Some people say that 96min is less than 80% of 210min so I can't; others say that PQR PWHT time shall be above the 80% of 96min,(mine it's 210min): so I can use.
I'm confused
.
Thanks
I have a PQR with PWHT time range of 210 min.
I have a WPS with PWHT of 96 min. (time range is the minimum required acc. to ASME VIII Div.1)
Welds are impact tested.
Question: may I use that PQR to cover this WPS? (assuming all other variables ok)
Some people say that 96min is less than 80% of 210min so I can't; others say that PQR PWHT time shall be above the 80% of 96min,(mine it's 210min): so I can use.
I'm confused
![[ponder] [ponder] [ponder]](/data/assets/smilies/ponder.gif)